Article
Short Communications
2018. V. 56. № 6. P. 936–937
Kostanovskii A.V., Zeodinov M.G., Kostanovskaya M.E., Pronkin A.A.
Thermal expansion of zirconium carbide at $1200$–$2850$ K
The results of an experimental study of the average coefficient of linear expansion of zirconium carbide in the temperature range $1200$–$2850$ K are presented. Samples of silicon carbide were prepared by the method of spark plasma sintering of zirconium carbide powder from nano sized particles at a temperature of $2100$ K.
Article reference:
Kostanovskii A.V., Zeodinov M.G., Kostanovskaya M.E., Pronkin A.A. Thermal expansion of zirconium carbide at $1200$–$2850$ K, High Temp., 2018. V. 56. № 6. P. 936
Kostanovskii A.V., Zeodinov M.G., Kostanovskaya M.E., Pronkin A.A. Thermal expansion of zirconium carbide at $1200$–$2850$ K, High Temp., 2018. V. 56. № 6. P. 936