Loading [MathJax]/jax/output/HTML-CSS/jax.js

Article

Thermophysical Properties of Materials
2018. V. 56. № 5. P. 685–688
Savinykh A.S., Garkushin G.V., Kanel' G.I., Razorenov S.V.
Evaluation of viscosity of BiPb melt (56.5%43.5%) by the width of a weak shock wave
Annotation
Experimental evaluation of the viscosity of 56.5%Bi43.5%Pb eutectic melt at 150С in a pressure range from 3 to 32 GPa on the basis of measurement of the shock wave width has been carried out. It was found that melt viscosity increases by 34 orders of magnitude under compression as compared to standard measurements at atmospheric pressure.
Article reference:
Savinykh A.S., Garkushin G.V., Kanel' G.I., Razorenov S.V. Evaluation of viscosity of BiPb melt (56.5%43.5%) by the width of a weak shock wave, High Temp., 2018. V. 56. № 5. P. 685