Article
Short Communications
2017. V. 55. № 6. P. 942–944
Kostanovskii A.V., Zeodinov M.G., Kostanovskaya M.E., Pronkin A.A., Borodina T.I.
Relative lengthening of ZrO2 in the temperature range of 1200–2700 K
Annotation
Results from the experimental investigation of the relative lengthening and mean thermal coefficient of the linear expansion of zirconium dioxide in the 1200–2700 K range are presented.
Article reference:
Kostanovskii A.V., Zeodinov M.G., Kostanovskaya M.E., Pronkin A.A., Borodina T.I. Relative lengthening of ZrO2 in the temperature range of 1200–2700 K, High Temp., 2017. V. 55. № 6. P. 942